Keywords

Recycled coarse aggregate, recycled concrete, splice length, concrete strain, flexural behavior

Document Type

Research Paper

Abstract

Interest in using recycled concrete aggregate (RCA) as a partial or full replacement for natural coarse aggregate (NCA) in concrete production has increased significantly in recent years. This shift contributes to reducing landfill usage and conserving natural resources. This study presents an experimental investigation into the behavior of sixteen rectangular beams cast with varying RCA ratios to examine the effects on ultimate load capacity and concrete strain. The beams, each measuring 1600 mm in length, 170 mm in width, and 260 mm in height, were reinforced with two longitudinal 12 mm steel bars, and 8 mm stirrups spaced at 75 mm intervals. The beams were categorized into four groups, with each group consisting of four beams containing RCA at replacement levels of 0%, 25%, 50%, and 75%, respectively. Group one beams were cast without rebar splice lengths, while the remaining three groups incorporated splice lengths of 10, 20, and 30 times the bar diameter (db), respectively. The experimental results indicate that RCA has a marginal impact on the ultimate load capacity. Specifically, for beams with a splice length of 10 db, RCA replacement at 25%, 50%, and 75% led to ultimate load reductions of 3.19%, 6.53%, and 11.7%, respectively. For beams with a 20 db splice length, the reductions were slightly lower at 2.78%, 5.05%, and 9.99%, respectively. In contrast, for beams with a 30 db splice length, the reductions were almost identical to those observed in beams without any splice length, measuring at approximately 1.59%, 2.82%, and 6.64%, respectively.

References

D. Mohammed, S. Tobeia, F. Mohammed, S. Hasan, Compressive strength improvement for recycled concrete aggregate, The 3rd International Conference on Buildings, Construction and Environmental Engineering, 162, 2018, 4-7. https://doi.org/10.1051/matecconf/201816202018 E. K. Sayhood, A. E. Al-Hamdani, J. K. Sahan, Effect of Recycled Aggregate on Behaviour of Tied and Spiral Reinforced Fibrous Circular Short Columns, Eng. Technol. J., 39 (2021) 1945-1952. http://doi.org/10.30684/etj.v39i12.965 M. A. Hadi, E. K. Sayhood, A. S. Resheq, Shear Strength of Reinforced Fibrous-self Compacted Concrete Box Girder using Recycled Concrete Aggregate, Eng. Technol. J., 39 (2021) 1307-1320. http://doi.org/10.30684/etj.v39i8.2100 F. Fiol, V. Revilla-Cuesta, M. Skaf, C. Thomas, J. M. Manso, Scaled Concrete Beams Containing Maximum Levels Of Coarse Recycled Aggregate: Structural Verifications For Precast-Concrete Building Applications, Struct. Concr., 24 (2023) 3476 - 3497. https://doi.org/10.1002/suco.202200963 N. A. Abdulla, Longitudinally Reinforced Recycled Aggregate Beams Without Transverse Steel: A Review, Discover Civil Eng., 1 (2024) 1-39.http://doi.org/10.1007/S44290-024-00048-0 S. B. Tobeia, M. M. Khattab, H. H. Khlaif, M. S. Ahmed, Enhancing recycled aggregate concrete properties by using polymeric materials, Mate. Today: Proc., 42 (2021) 2785 - 2788. https://doi.org/10.1016/j.matpr.2020.12.722 E. K. Sayhood, A.S. Resheq, F. L. Raoof, Behavior of Recycled Aggregate Fibrous Reinforced Beams Under Flexural and Shear Loading, Eng. Technol. J., 37 (2019) 338 - 344. https://doi.org/10.30684/etj.37.3C.6 E. E. Anike, M. Saidani, A. O. Olubanwo, U. C. Anya, Flexural performance of reinforced concrete beams with recycled aggregates and steel fibres,Structures, 39 (2022) 1264-1278. https://doi.org/10.1016/j.istruc.2022.03.089 M. H. Harajli, K. A. Salloukh, Effect of fibers on development/splice strength of reinforcing bars in tension, Mater. J., 94 (1997) 317–324. Wu. Chenglin, G. Chen, J.S. Volz, R. K. Brow, M. L. Koenigstein, Global bond behaviour of enamel-coated rebar in concrete beams with spliced reinforcement, Constr. Build. Mater., 40 (2013) 793-801. https://doi.org/10.1016/j.conbuildmat.2012.11.076 E. Kadhem, A. A. Ali, Bond Stress-Slip Relationship in Reactive Powder Concrete Beams, Int. J. Civil, Eng. Technol., 9 (2018) 1078-1089. H. M. Al-Hassani, Q. A. M. Hassan, F. F. Saleem, Effect of lap splicing high tensile steel bars in reactive powder concrete beams exposed to repeated loading, J. Eng. Sustain. Dev., 21 (2017) 47-59. BIS (Bureau of Indian Standards), I.S. 8112. 43 Grade ordinary Portland cement – Specification, Bureau of Indian Standards, New Delhi, India, 1989 (Reaffirmed, 2005). BIS (Bureau of Indian Standards), I.S. 383, "Specification for coarse and fine aggregates from natural sources for concrete", Bureau of Indian Standards, New Delhi, India, 1970 (Reaffirmed 2002). http://refhub.elsevier.com/S0950-0618(17)32214-6/h0120. ASTM C33/C33M − 11, “Standard Specification for Concrete Aggregates1,” vol. i, no. C, pp. 1–11, 2010, doi: 10.1520/C0033. S. Nagataki, A. Gokce, T. Saeki, M. Hisada, Assessment of recycling process induced damage sensitivity of recycled concrete aggregates, Cem. Concr. Res., 34 (2004) 965 - 971. https://doi.org/10.1016/j.cemconres.2003.11.008 BIS (Bureau of Indian Standards), IS 2386(Part IV), "Methods of test for aggregates for concrete – Part IV Mechanical properties", Bureau of Indian Standards New Delhi, India, 1963 (Reaffirmed 2007). ASTM C33/C33M − 11, “Standard Specification for Concrete Aggregates1,” vol. i, no. C, pp. 1–11, 2010, doi: 10.1520/C0033. ASTM, C1240-03 , “Standard specification for silica fume used in cementitious mixtures”, USA: American Society for Testing Materials, 9. 2003, http://www.microsilica-fume. ASTM A615/A615M, “Standard specification for deformed and plain carbon-steel bars for concrete reinforcement”, ASTM International, West Conshohocken, 2009, https://www.astm.org/a0615_a0615m-09.html ACI Committee 408, “ACI 408R-03 Bond and Development of Straight Reinforcing Bars in Tension,” American Concrete Institute, pp. 1–49, 2003. M. Harajli, M. Abouniaj, Bond performance of GFRP bars in tension: Experimental and assessment of ACI 440 guidelines, J. Compos. Constr., 14 (2010) 659-668. https://doi.org/10.1061/(ASCE)CC.1943-5614.0000139 ACI 318: Building code requirements for structural concrete and commentary, 318, American Concrete Institute, 2019 (Reaffirmed 2022). International Federation for Structural Concrete - FIB, Model Code for Concrete Structures 2010. Bulletin No 52 Fib, 2, Lausanne, Switzerland, 2012. V.W.Y. Tam, D. Kotrayothar, J. Xiao, Long-term deformation behaviour of recycled aggregate concrete, Constr. Build. Mater., 100) 2015) 262-272. https://doi.org/10.1016/j.conbuildmat.2015.10.013 J. Eiras-Lopez', S. Seara-Paz, B. Gonz'alez-Fonteboa, F. Martínez-Abella, Bond behaviour of recycled concrete. Analysis and prediction of bond stress-slip curve, J. Mater. Civ. Eng., 29 (2017). https://doi.org/10.1061/(ASCE)MT.1943-5533.0002000 S.Seara-Paz, B.Gonzalez-Fonteboa, J. Eiras-Lopez, MF. Herrador, Bond behaviour between steel reinforcement and recycled concrete, Mater. Struct., 47 (2014) 323-334. http://dx.doi.org/10.1617/s11527-013-0063-z J. Xiao, H. Falkner, Bond behaviour between recycled aggregate concrete and steel rebars, Constr. Build. Mater., 21 (2007) 395- 401. https://doi.org/10.1016/j.conbuildmat.2005.08.008 S .Seara-Paz, B. Gonz'alez-Fonteboa, F. Martínez-Abella, J. Eiras-Lopez , Flexural performance of reinforced concrete beams made with recycled concrete coarse aggregate, Eng. Struct., 156 (2018) 32- 45. https://doi.org/10.1016/j.engstruct.2017.11.015

Highlights

Flexural tests involve sixteen beams with varying recycled coarse aggregate ratios and different lap splice lengths. Beams containing RCA exhibit behavior similar to those without RCA. The load-bearing capacity declines as the RCA content in the concrete mix increases. An RCA ratio of 50% is more suitable compared to other ratios. Concrete strain distribution across the beam cross-section decreases with higher RCA

DOI

10.30684/etj.2024.153907.1823

First Page

270

Last Page

282

Share

COinS